MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borlink™ LE0592 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE0592 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications: LE0592 is intended for semi conductive applications in XLPE medium and high voltage cables. It can be used as inner and outer semicon for bonded constructions and as inner semicon for strippable constructions. Specifications: AEIC CS7; AEIC CS8; BS 6622; DIN VDE 0276-620; DIN VDE 0276-263; HD 620 S1; HD 632 S1; IEC 60502; IEC 60840; ISO 1872-E/BA, KHXY, 23-G200, C40; NF C33-223; NF C33-226; UTE C 33-223; UTE C 33-223; and ICEA S-93-639.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.135 g/cc0.04100 lb/in³ISO 1183/ISO 1872-2
Water Absorption 0.030 %0.030 %Karl Fischer-titration
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 4.40 MPa<= 638 psiafter aging (240h, 135°C); IEC 60811-1-2
 22.0 MPa3190 psi25mm/min; ISO 527
Elongation at Break 200 %200 %25mm/min; ISO 527
Tensile Set 0.00 %
@Temperature 200 °C
0.00 %
@Temperature 392 °F
Permanent Deformation at 0.2 MPa after 25% elongation under load; IEC 60811-2-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  <= 100 ohm-cm
@Temperature 23.0 °C
<= 100 ohm-cm
@Temperature 73.4 °F
ISO 3915
 <= 1000 ohm-cm
@Temperature 90.0 °C
<= 1000 ohm-cm
@Temperature 194 °F
ISO 3915
 
Processing PropertiesMetricEnglishComments
Melt Temperature 120 - 140 °C248 - 284 °F
Drying Temperature 60.0 °C140 °Fhopper drying
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Göttfert Elastograph (Nm)1.14-1.38

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borlink™ LS4201S Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE4244EHV Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE4201EHV Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE0511 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Borlink™ LE0500 Crosslinkable Semiconductive Shielding Compound

PBOREA512 / 108771

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.