MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay Engineered Polymers DEXFLEX® 711-300 TPO  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: DEXFLEX® 711-300 is a thermoplastic olefinic elastomer compound with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched) black, and that require very good processing characteristics.

Applications: Wheel liners, filler panels, fan shrouds, air dams, and sight shields

Information provided by Solvay Engineering Polymers

LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm0.0090 - 0.011 in/inASTM D995
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.3 MPa2510 psi2 in/min, Type 1; ASTM D638
Flexural Modulus 1.52 GPa220 ksi0.05 in/min, 1x3"; ASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 71.0 µm/m-°C
@Temperature 20.0 °C
39.4 µin/in-°F
@Temperature 68.0 °F
modified; ASTM D696

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell DEXFLEX® 711 TPO
LyondellBasell Dexflex 711-300 BLK Thermoplastic Polyolefin
Celanese SO.F.TER Sofprene® Eco-Friendly 38 E SBS TPE Foot Ware Compound
Celanese SO.F.TER Sofprene® Eco-Friendly 12 SE SBS TPE Foot Ware Compound
Buckeye Polymers BP FLEX 8000 VP BLK Thermoplastic Elastomer TPV

PSOLH12 / 68067

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.