MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bamberger Polymers Bapolene® 107B Low Density Polyethylene Film Extrusion Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Bapolene® 107B is a low density polyethylene for blown film. This product meets the Food and Drug Administration requirements of 21CFR177.1520.

Applications: Bags; Blown Film; Film; Food Packaging; General Purpose; Packaging

Information provided by Bamberger Polymers.

Key Words: Food Contact Acceptable; Low Density
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D-1505
Thickness 50.8 microns2.00 milBlow ratio to 2.5:1
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Elmendorf Tear Strength MD 170 g170 gASTM D1922
Elmendorf Tear Strength TD 130 g130 gASTM D1922
Dart Drop Test 150 g0.331 lbASTM D1709
Film Tensile Strength at Break, MD 29.0 MPa4200 psiASTM D882
Film Tensile Strength at Break, TD 20.0 MPa2900 psiASTM D882
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processBlown Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Bamberger Polymers Bapolene® 105F Low Density Polyethylene Film Resin
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Bamberger Polymers Bapolene® 108A Low Density Polyethylene Film Extrusion Resin

PBP3B370Cf / 172252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.