MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Sanfor® G/35 35% Glass Fiber Reinforced SAN
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded, Glass Reinforced

Material Notes: Excellent rigidity and dimensional stability. Natural and colored PP based compound. U.L. approved for automotive, electrical, appliances, tools, and other industrial parts. These compounds are used mainly in the automotive and household industry to manufacture outer casings and protection guards, in the furniture sector to manufacture chairs, for the production of footwear, and for the production of sport articles such as helmets, ski boots, and roller blades.

Information provided by SO.F.TER. Spa

Key Words: Softer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D1505, ISO 1183
Water Absorption 0.10 %0.10 %24 hours; ASTM D570, ISO 62
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 110 MPa16000 psiASTM D638, ISO 527
Elongation at Break 1.5 %1.5 %ASTM D638, ISO 527
Flexural Modulus 9.50 GPa1380 ksiASTM D790, ISO 178
Izod Impact, Unnotched 0.400 J/cm0.749 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FASTM D648, ISO 75
Vicat Softening Point 108 °C226 °F49N/50; ASTM D1525, ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °FCylinder Temperature
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3 hour3 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram RamShine PW300G7 SAN, 35% Glass Fiber
Polykemi AB POLYsan FL100 F35 SAN, Glass Fiber-Reinforced
Lotte Advanced Materials Starex® GR-5020T SAN, 20% Glass Filled
INEOS Styrolution Absolan® 25GF30%
Daicel CEVIAN®-N GRSJ3 30% GF SAN resin

PSOFT37 / 67911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.