System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical Lupox® SV1120M PBT
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
Description: Injection Molding, PBT, General Purpose, High Viscosity
Application: Films & Sheets, Optical Loose Tube
CAS No. 65997-17-3 and 24968-12-5
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.31
g/cc
1.31
g/cc
ASTM D792
Water Absorption
0.080 %
@Temperature 23.0 °C,
Time 86400 sec
0.080 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Maximum Moisture Content
0.020
0.020
Injection Molding
Linear Mold Shrinkage, Flow
0.018
-
0.021
cm/cm
@Thickness 3.20 mm
0.018
-
0.021
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
10
g/10 min
@Load 2.16 kg,
Temperature 260 °C
10
g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
47.1
MPa
@Thickness 3.20 mm
6830
psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break
>= 200 %
@Thickness 3.20 mm
>= 200 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength
83.4
MPa
@Thickness 3.20 mm
12100
psi
@Thickness 0.126 in
2.8mm/min; ASTM D790
Flexural Modulus
2.45
GPa
@Thickness 3.20 mm
356
ksi
@Thickness 0.126 in
2.8mm/min; ASTM D790
Izod Impact, Notched
0.392
J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
0.735
ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Melting Point
225
°C
437
°F
@ Break; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
154
°C
@Thickness 6.40 mm
309
°F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
57.0
°C
@Thickness 6.40 mm
135
°F
@Thickness 0.252 in
Unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
230
-
240
°C
446
-
464
°F
Injection Molding
Middle Barrel Temperature
240
-
250
°C
464
-
482
°F
Injection Molding
Front Barrel Temperature
250
-
260
°C
482
-
500
°F
Injection Molding
Nozzle Temperature
250
-
260
°C
482
-
500
°F
Injection Molding
Mold Temperature
40.0
-
80.0
°C
104
-
176
°F
Injection Molding
Drying Temperature
100
-
120
°C
212
-
248
°F
Injection Molding
Dry Time
3.00
-
5.00
hour
3.00
-
5.00
hour
Injection Molding
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Overview of materials for Acetal Homopolymer, PTFE-Filled
Overview of materials for ABS/Polyester Alloy
LG Chemical Lupox® TE5000D PBT+PC
LG Chemical Lupox® SG3180S PBT+PET+MF18%
LG Chemical Lupox® LW5402A PBT+PC+GF40%
PLAY293 / 148303
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.