MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® CP-0301 Fiber Compound
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: The sheet molding compound series of Vespel® CP parts consist of long, chopped fibers held in a variety of polymer matrices. The discontinuous nature of the fibers allows the fibers to align with the contours of the part, permitting the molding of relatively complex shapes, while providing the reinforcing strength where needed within the part. Superior strength versus aluminum at less weight, Vespel® CP frees the designer to explore ways to improve efficiency by reducing component weight and reducing friction.

Applications: A sheet-molded and reinforced polyimide resin for:

  • Tube clamps
  • Brackets
  • Seal plates
  • Gear box adapter covers

Benefits:
  • Lightweight yet tough: ideal for replacing cast aluminum or titanium
  • Polymer base may be made from phenolics and / or polyimides

All values listed are for compression-molded samples and are measured in the plane perpendicular to the direction of molding pressure unless otherwise indicated.

Information provided by DuPont

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccASTM D792
Water Absorption 0.50 %0.50 %24 hrs @ 73°F (23°C); ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 15T 8686ASTM D2240
Tensile Strength, Ultimate 345 MPa50000 psiRT; ASTM D3039
 324 MPa
@Temperature 260 °C
47000 psi
@Temperature 500 °F
ASTM D3039
Tensile Modulus 45.0 GPa6530 ksi260°C (500°F); ASTM D3039
 46.9 GPa6800 ksiRT; ASTM D3039
Flexural Strength 345 MPa50000 psi260°C (500°F); ASTM D790
 490 MPa71000 psiASTM D790
Flexural Modulus 33.1 GPa4800 ksi260°C (500°F); ASTM D790
 37.9 GPa5500 ksiRT; ASTM D790
Compressive Strength 241 MPa35000 psiUltimate; 260°C (500°F); Parallel to the direction of molding pressure.; ASTM D695
 365 MPa53000 psiUltimate; RT; Parallel to the direction of molding pressure.; ASTM D695
Izod Impact, Notched 6.94 J/cm13.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear  2.88 µm/m-°C
@Temperature 21.1 - 316 °C
1.60 µin/in-°F
@Temperature 70.0 - 600 °F
ASTM D696
 27.0 µm/m-°C
@Temperature 21.1 - 316 °C
15.0 µin/in-°F
@Temperature 70.0 - 600 °F
ASTM E228-85
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FASTM C177
Glass Transition Temp, Tg 335 °C635 °F
 
Descriptive Properties
Thermal Oxidation, % Weight Loss10410 hours; 70 psia (483 kPa) 610°F (321°C) circulating air; saturated condition; volume/surface area .07 in
 2.5120 hours; 70 psia (483 kPa) 610°F (321°C) circulating air; saturated condition; volume/surface area .07 in
 4100 hours; 70 psia (483 kPa) 610°F (321°C) circulating air; saturated condition; volume/surface area .048 in (1.22 mm)
 7.5315 hours; 70 psia (483 kPa) 610°F (321°C) circulating air; saturated condition; volume/surface area .07 in
Thermal Oxidative Stability, %2100 hours; 70 psia (483 kPa) 610°F (321°C) circulating air; saturated condition; volume/surface area .091 in (2.31 mm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled
DuPont Mobility and Materials Vespel® SCP-50094 Polyimide
DuPont Mobility and Materials Vespel® SMP-40025 DF Polyimide
DuPont Mobility and Materials Vespel® SP-202 Conductive Polyimide
Overview of materials for Nylon 46, Glass Fiber Reinforced

PDU2043 / 32908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.