MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® DP 1802 H3.0 000000 Nylon 6 (PA6), Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: PA 6, non-reinforced, impact-modified, halogen-free

Extrusion grade for corrugated tubes, electrical and building applications

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Water Absorption at Saturation 8.0 %8.0 %IOS 62
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 110 MPa16000 psiISO 2093-1
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ISO 527-1,-2
Elongation at Yield 3.9 %3.9 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 80.0 MPa11600 psi2 mm/min; ISO 178-A
Flexural Yield Strength 75.0 MPa
@Strain 3.5 %
10900 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 5.5 %5.5 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched 12.5 J/cm²
@Temperature 23.0 °C
59.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 156 °C313 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °FISO 75-1,-2
Vicat Softening Point 185 °C
@Load 5.10 kg
365 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8351 HS BK 106 PA6 (Dry)
BASF Ultramid® 8351 HS BK 102 PA6 (Dry)

PLANW9502 / 208317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.