MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Weartech International WT-50 Nickel Hardfacing & Wear Resistant Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Applications: liners, thrust shoes, bushings, cages and other valve components for nuclear applications

Information provided by Weartech International

Key Words: RNiCr-B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.14 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 45 - 5645 - 56
Hardness, Vickers  100
@Treatment Temp. 760 °C
100
@Treatment Temp. 1400 °F
 250
@Treatment Temp. 649 °C
250
@Treatment Temp. 1200 °F
 450
@Treatment Temp. 427 °C
450
@Treatment Temp. 800 °F
 480
@Treatment Temp. 538 °C
480
@Treatment Temp. 1000 °F
 525
@Treatment Temp. 25.0 °C
525
@Treatment Temp. 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.1 µm/m-°C8.40 µin/in-°F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Melting Point <= 1070 °C<= 1950 °F
Liquidus 1070 °C1950 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 3.0 %3.0 %
Carbon, C 0.60 %0.60 %
Chromium, Cr 13 %13 %
Iron, Fe 4.0 %4.0 %
Nickel, Ni 75.7 %75.7 %
Silicon, Si 3.7 %3.7 %
 
Descriptive Properties
Relative Wear PerformanceCold AbrasionExcellent
 CorrosionGood/Moderate
 ErosionGood/Moderate
 Hot AbrasionGood/Moderate
 ImpactNot Recommended
 Metal to MetalExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Weartech International WT-60 Nickel Hardfacing & Wear Resistant Alloy

NWEART020 / 142557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.