MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:
  • Available in North America
  • UV Stabilizer
  • Good Toughness
  • Low Gloss
  • RoHS Compliant
  • Form: Pellets
  • Processing Method: Injection Molding
  • Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: BD1 LT GREYSTONE Gray 632, GM GMP.ABS+PC.017 Color: All Color Matches

Information provided by Ravago

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955 and ISO 294-4
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 260 °C
15 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.7 MPa7500 psiASTM D638
 52.0 MPa7540 psiISO 527-2
Elongation at Break 55 %55 %ASTM D638
 55 %55 %ISO 527-2
Flexural Yield Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.21 GPa320 ksiASTM D790
 2.23 GPa323 ksiISO 178
Izod Impact, Notched 5.34 J/cm10.0 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 37.8 kJ/m²18.0 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FUnannealed; ASTM D648
 112 °C234 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 243 °C450 - 470 °F
Middle Barrel Temperature 238 - 260 °C460 - 500 °F
Front Barrel Temperature 243 - 271 °C470 - 520 °F
Nozzle Temperature 243 - 271 °C470 - 520 °F
Mold Temperature 65.6 - 82.2 °C150 - 180 °F
Drying Temperature 104 - 110 °C
@Time 7200 - 14400 sec
220 - 230 °F
@Time 2.00 - 4.00 hour
Dry Time <= 10.0 hour<= 10.0 hour
Moisture Content <= 0.040 %<= 0.040 %Suggested Maximum
Injection Pressure 5.52 - 12.4 MPa800 - 1800 psi
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
Shot Size 40 - 80 %40 - 80 %
Screw Speed 40 - 60 rpm40 - 60 rpm
 
Descriptive Properties
Injection RateModerate
Melt-Volume Flow Rate, 260°C/5.0 kg (in3/10 min)0.854ISO 1133

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Echo® RPEHD BK HDPE
Ravago Manufacturing Americas Hysun™ 693 ASA
Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS
Lotte Advanced Materials Infino® LS-1159S PC/ABS/ 15% GF, High Impact
LG Chemical LUPOY HR5007AE PC/ABS, High Impact

PENTA008b / 142654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.