MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 230 PA6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.

Available in: Europe

Product Applications: This grade has improved impact strength and higher flexibility. It is suitable specially to make technical parts having small or medium size, such as: plugs, seals. This product is available in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.0 MPa5660 psiISO 527 type 1 A
Tensile Modulus 1.00 GPa145 ksiISO 527 Type 1A
Flexural Strength 35.0 MPa5080 psiISO 178
Flexural Modulus 0.800 GPa116 ksiISO 178
Izod Impact, Notched (ISO) 82.0 kJ/m²39.0 ft-lb/in²ISO 180/1eA
Charpy Impact, Notched 9.00 J/cm²42.8 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Constant 4.04.0IEC 60250
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243
Dissipation Factor 0.120.12IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Dry)
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Quantum Composites AMC™ 2593 45% Carbon Fiber Reinforced Phenolic SMC
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP
Domo TECHNYL® C 216 V30 Black Z/4 PA 6 30% Glass Reinforced, Conditioned

PRHOD778 / 138009

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.