MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NAECO® ELKON® 3150 Silver Tungsten Carbide contact material ASTM B663 Table 2, Class B
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Precious Metal; Silver Alloy; Tungsten Alloy

Material Notes: For arcing and current carrying electrical contacts resistant to welding and sticking.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.93 g/cc0.4310 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6060
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000383 ohm-cm0.00000383 ohm-cm(45% IACS)
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 175 W/m-K1210 BTU-in/hr-ft²-°F
Melting Point >= 980 °C>= 1800 °F
Solidus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 50 %50 %
WC 50 %50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NAECO® ELKON® 3042 Silver Tungsten Carbide contact material ASTM B663
NAECO® ELKON® 1060 Silver Tungsten Carbide Contact Material
NAECO® ELKON® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated
CMW® ELKONITE® 1060 Silver Tungsten Carbide Contact Material
NAECO® ELKON® 2150 Silver Tungsten contact material ASTM B631, Class C, press-sinter-repress

NCMV840 / 192425

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.