Characteristics: Control reologhy high melt flow rate narrow molecular weight distribution Homopolymer polypropylene, lot to lot consistency, with special additives package and high cleanness, to get stable spinning processability in low denier fiber at high speed, good gas fading resistant. Recommended for: Fabrication of Non woven fabrics by high speed Spunbond process, melt spinning of low denier fibers, extrusion coating of raffia woven fabrics, general purpose injection molding applications. Information provided by Esenttia by Propilco |