Elastomer Engineering E900-90A Polyurethane
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
;
Thermoplastic Polyurethane (TPUR), Polyester Grade
Material Notes:
A polyether-based urethane that is excellent in water treatment applications. Typical uses: Wheels, casters, rolls, metal forming strippers and pads.
Information provided by Elastomer Engineering Inc (EEI)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
90
90
Tensile Strength, Ultimate
44.8
MPa
6500
psi
Elongation at Break
430 %
430 %
100% Modulus
7.58
MPa
@Strain 100 %
1100
psi
@Strain 100 %
300% Modulus
15.2
MPa
@Strain 300 %
2200
psi
@Strain 300 %
Rebound
42 %
42 %
Bayshore
Tear Strength
12.3
kN/m
70.0
pli
D-470
Compression Set
25 %
25 %
Method B
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
Lanxess Addocat® 201 PU Catalyst/Activator
RTP Company ESD C 1200-90A Polyurethane Elastomer (TPU) Conductive - 90 Shore A
Dow BETAMATE™ 7205 Polyurethane Prepolymer
Dow BETAMATE™ 7201 Polyurethane Prepolymer
PELAS04 / 35676
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.