MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes: PC/ABS Alloy, General Purpose, 30% Glass Filled

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inASTM D955
Melt Flow 1.0 - 10 g/10 min
@Load 5.00 kg,
Temperature 250 °C
1.0 - 10 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 82.7 MPa12000 psiASTM D638
Tensile Strength, Yield 82.7 MPa12000 psiASTM D638
Flexural Strength 131 MPa19000 psiASTM D790
Flexural Modulus 6.21 GPa900 ksiASTM D790
Izod Impact, Notched 0.694 J/cm
@Temperature 22.8 °C
1.30 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C265 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 288 °C480 - 550 °F
Middle Barrel Temperature 254 - 293 °C490 - 560 °F
Front Barrel Temperature 260 - 302 °C500 - 575 °F
Melt Temperature 271 - 299 °C520 - 570 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 79.4 - 85.0 °C175 - 185 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00381 cm0.00150 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Plastiblend® PC/ABS FR GF30 30% Glass Filled
Covestro Bayblend® FR1514 PC/ABS Blend
Daicel CEVIAN® S5230 30% GF PC/ABS alloy
Mitsubishi Iupilon® MB 1700 PC/ABS
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend

PPOLYQ088 / 160604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.