MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLTHANE® CLEAR 15N70 combines low hardness and high elasticity with excellent mechanical properties and excellent hydrolysis resistance. It can be extruded and injection-molded.

Information provided by Merquinsa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272ISO 868
Tensile Strength, Yield 30.1 MPa4360 psiISO 527-2/5A/500
Elongation at Break 710 %710 %ISO 527-2/5A/500
100% Modulus 3.01 MPa
@Strain 100 %
436 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 5.01 MPa
@Strain 300 %
727 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 64.9 kN/m370 pliUnnicked; ISO 34-1B
Abrasion 2525Resistance, mm3; ISO 4649-A
 
Processing PropertiesMetricEnglishComments
Zone 1 170 - 190 °C338 - 374 °F
Zone 2 180 - 205 °C356 - 401 °F
Zone 3 190 - 215 °C374 - 419 °F
Zone 4 180 - 190 °C356 - 374 °F
Adapter Temperature 185 - 190 °C365 - 374 °F5
Die Temperature 185 - 190 °C365 - 374 °F(6)
 185 - 190 °C365 - 374 °FTIP (7)
Drying Temperature 100 °C
@Time 7200 sec
212 °F
@Time 2.00 hour
Dew Point <= -30.0 °C<= -22.0 °F
 
Descriptive Properties
Compression Zone190°C
Metering Zone200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer

PMER65 / 52866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.