MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.

Main Applications: Greenflex HN 70 is recommended as base component for hot melt adhesives used in packaging, bookbinding and woodworking.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.952 g/cc0.952 g/ccISO 1183
Vinyl Acetate Content 28 %28 %Internal Method
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575ISO 868/A
Hardness, Shore D 3131ISO 868/A
Tensile Strength, Yield 2.70 MPa392 psiISO 527
Flexural Modulus 0.0150 GPa2.18 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 73.0 °C163 °FInternal Method
Vicat Softening Point 45.0 °C
@Load 1.00 kg
113 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -80.0 °C<= -112 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Eurofoam Evacell EVA 30 EVA + PE Foam
LyondellBasell Ultrathene® UE637000 Ethylene Vinyl Acetate Copolymer, Film Extrusion Grade
Versalis Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion
Eurofoam Evacell EVA 100 EVA + PE Foam

PENG153 / 124547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.