MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Inno-Comp INNOPOL® CS 1-3000 B DEL Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: INNOPOL® CS 1-3000 B DEL is developed for producing injection molded automotive components.

All information provided by INNO-COMP.

Key Words: PP-H
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc
@Temperature 23.0 °C
0.0332 lb/in³
@Temperature 73.4 °F
ISO 1183
Linear Mold Shrinkage, Flow 0.0117 cm/cm0.0117 in/inISO 294
Linear Mold Shrinkage, Transverse 0.0096 cm/cm0.0096 in/inISO 294
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 36.0 MPa5220 psi50 mm/min; ISO 527-1,-2
Elongation at Break 14 %14 %ISO 527-1,-2
Elongation at Yield 8.0 %8.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1.65 GPa239 ksi1 mm/min; ISO 527-1,-2
Flexural Modulus 1.80 GPa261 ksi2 mm/min; ISO 178
Charpy Impact Unnotched  1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.120 J/cm²
@Temperature -30.0 °C
0.571 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.370 J/cm²
@Temperature 23.0 °C
1.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 162 °C324 °FDSC; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C129 °FISO 75-1,-2
Vicat Softening Point 94.0 °C201 °FB120; ISO 306
 153 °C307 °FA120; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
FMVSS 302
 
Descriptive Properties
Automotive MaterialsPassFMVSS 302
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Inno-Comp INNOPOL® CS 1-3130 30% Talc-Filled Polypropylene Homopolymer
Inno-Comp INNOPOL® CS 1-8000 Polypropylene Homopolymer
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer
Inno-Comp INNOPOL® CS 1-3140 40% Talc-Filled Polypropylene Homopolymer

PINNO005 / 82666

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.