Total Petrochemicals Polystyrene 3341 is a high impact polystyrene for the extrusion industry. Its good mechanical and thermal properties leads to the production of thermoformed articles of good rigidity and toughness. Applications: - Sheet for thermoforming
- Industrial sheet
Information provided by Total Petrochemicals. |