MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Bond 286-5 Latex Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: TRA-BOND 286-5 latex emulsion is designed for temporary sealing of molds to prevent leaking during cure. This compound will thicken gradually due to water evaporation. Store containers with caps securely sealed.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 20000 cP
@Temperature 25.0 °C
20000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2323
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 75.0 °C
4.00 hour
@Temperature 167 °F
 1440 min
@Temperature 55.0 °C
24.0 hour
@Temperature 131 °F
Shelf Life 1.00 Month1.00 MonthAt 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories CFA-2 Ceramic Foam
Mafic Direct Basalt Roving 10 µm Diameter
LG Chemical Lutex 703 SBR Latex
KKPC KOSYN KSL 601 Styrene-Butadiene Latex
Hexcel® HexTow® AS4A Standard Modulus Carbon Fiber (12,000 Filaments)

PTRAC076 / 71004

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.