MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Neoprene AD-20 Polychloroprene Rubber  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development. More color-stable than neoprene AC during storage.

Processing and Performance Features:

  • Primary use is in contact adhesives that require high initial and ultimate bond strength and ability to form bonds with minimum pressure after long open assembly periods
  • Neoprene AD can be dissolved without milling, or can be milled before solution (for rheology control), to cover a broad range of solution viscosity. It is soluble in solvents with various evaporation rates
  • Compounded adhesives can be stored in iron containers without the discoloration experienced with compounds based on Neoprene AC.

Information provided by manufacturer.

Denka Performance Elastomer LLC has acquired the Neoprene product line from DuPont Performance Polymers. This specific product had already been discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Brookfield Viscosity 3.50e+7 - 5.30e+7 cP
@Temperature 25.0 °C
3.50e+7 - 5.30e+7 cP
@Temperature 77.0 °F
6 rpm or 3 rpm depending on viscosity
 
Descriptive Properties
Crystallization RateRapid
Physical Form and ColorWhite to light yellow chips; discolors in light
Polymer TypeChloroprene homopolymer
SolubilitySolublein aromatic hydrocarbons and mixtures with esters, ketones, aliphatic hydrocarbons, and selected chlorinated solvents
StabilityExcellentstorage at temperatures below 21°C will retard darkening of color and gradual increase in viscosity.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka Neoprene 671A Polychloroprene
Denka Neoprene 750 Copolymer of chloroprene and 2,3,dichloro-1,3,-butadiene
DuPont Mobility and Materials Neoprene 571 Polychloroprene
DuPont Mobility and Materials Neoprene 671A Polychloroprene
DuPont Mobility and Materials Neoprene 842A Polychloroprene

PDVE22 / 34064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.