MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 86B30H Steel, water quenched 845°C (1550°F), 540°C (1000°F) temper, 100 mm (4 in.) round
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Water quenched 845°C (1550°F), 540°C temper, 100 mm round. Post water quenched hardness 47 HRC surface, 25 HRC half-radius, 22 HRC center

Key Words: UNS H86301, ASTM A304, SAE J1268
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217217
Hardness, Knoop 240240Converted from Brinell
Hardness, Rockwell B 9595Converted from Brinell
Hardness, Rockwell C 1717Converted from Brinell hardness. Value below normal HRC range, for comparison only.
Hardness, Vickers 228228Converted from Brinell
Tensile Strength, Ultimate 738 MPa107000 psi
Tensile Strength, Yield 565 MPa81900 psi
Elongation at Break 23 %23 %in 50 mm
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Calculated
Machinability 70 %70 %annealed and cold drawn. Based on AISI 1212 steel = 100%.
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000234 ohm-cm0.0000234 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.2 µm/m-°C
@Temperature 21.0 - 100 °C
6.22 µin/in-°F
@Temperature 69.8 - 212 °F
 12.2 µm/m-°C
@Temperature 21.0 - 200 °C
6.78 µin/in-°F
@Temperature 69.8 - 392 °F
 14.0 µm/m-°C
@Temperature 21.0 - 500 °C
7.78 µin/in-°F
@Temperature 69.8 - 932 °F
Specific Heat Capacity 0.475 J/g-°C0.114 BTU/lb-°FTypical steel
Thermal Conductivity 46.6 W/m-K323 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.00050 - 0.0030 %0.00050 - 0.0030 %
Carbon, C 0.27 - 0.33 %0.27 - 0.33 %
Chromium, Cr 0.35 - 0.65 %0.35 - 0.65 %
Iron, Fe 96.692 - 98.0795 %96.692 - 98.0795 %As remainder
Manganese, Mn 0.65 - 0.95 %0.65 - 0.95 %
Molybdenum, Mo 0.15 - 0.25 %0.15 - 0.25 %
Nickel, Ni 0.35 - 0.75 %0.35 - 0.75 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 8620 Steel, normalized, machined to 25 mm, pseudocarburized, reheated to 800°C, 150°C temper
AISI 8620 Steel, normalized, machined to 13.7 mm, pseudocarburized, reheated to 800°C, 150°C temper
AISI 8620 Steel, carburized, box cooled, reheated and quenched, 150°C (300°F) temper, 50 mm (2 in.) round
AISI 8620 Steel, carburized, box cooled, reheated and quenched, 150°C (300°F) temper, 25 mm (1 in.) round
AISI 8620 Steel, carburized, box cooled, reheated and double quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round

M863CS / 8451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.