MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.

Available in: Europe, Latin America and North America

Product Applications: In addition to primary polyamide properties, TECHNYL ® A 238 V13 offers a very good rigidity/impact resistance compromise, at high temperatures. This grade is used for under bonnet automotive parts, such as: various covers and fasteners. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage 0.0085 cm/cm0.0085 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0085 cm/cm0.0085 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiISO 527 type 1 A
Elongation at Yield 4.0 %4.0 %ISO 527 type 1 A
Tensile Modulus 5.50 GPa798 ksiISO 527 Type 1A
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 6.50 J/cm²30.9 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 228 °C442 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 270 - 280 °C518 - 536 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 238 V13 PA66, 13% glass fiber, Conditioned
Domo TECHNYL® A 238 Black 21 N PA66, DRY
Domo TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Conditioned)
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry)

PRHOD695 / 137926

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.