MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAFAC® LO-529 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Moderate foamer. Water and solvent soluble. Imparts good hard surface detergency. Retards corrosion. Adds water rinsability to paint strippers. Prolongs life of floor finishes. Dry cleaning detergent. Antistat for acrylic carpet fiber. Useful in waterless hand cleaners and polymerization.

Identification: Nonylphenol Ethoxylate, Partial Sodium Salt

CAS: 68954-84-7

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAFAC LO-529 is a detergent, foamer, corrosion inhibitor, emulsifier for detergent concentrates, metalworking fluids, FDA, EPA compliance. Pigment dispersing agent for paint coloring.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 5.0 - 5.85.0 - 5.810% Solution; RP-0402
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 10 - 13 %10 - 13 %RP-0327
 
Descriptive Properties
AppearanceClear viscous liquidRP-0064
Color<100APHA, RP-0134
CompositionNonionic Content30-35%, RP-0351

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAFAC® RS-610 Surfactant
Solvay RHODAFAC® LO/529-E Surfactant
Solvay RHODACAL® 60/B Surfactant
Solvay RHODACAL® 60/BE Surfactant
Solvay RHODAFAC® RE-610 E Surfactant

WRHOD354 / 137585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.