MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Xantar® C CM 546 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: XANTAR® C properties are: Highest flow in combination with excellent toughness. High level of purity. High stability. Bright natural color. The benefits are: easier filling of complex parts, lower mould deposit during injection molding, low volatiles level and reduced fogging tendency, better long-term property retention and improved color consistency and appearance.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³
Moisture Absorption 0.200 %0.200 %
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0030 cm/cm0.0030 in/in
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 260 °C
10 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm³/10 min Volumetric Rate
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi
Tensile Strength, Yield 55.0 MPa7980 psi
Tensile Modulus 6.00 GPa870 ksi
Flexural Strength 95.0 MPa13800 psi
Flexural Modulus 5.50 GPa798 ksi
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Comparative Tracking Index 175 - 250 V175 - 250 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °F
Vicat Softening Point 131 °C
@Load 5.10 kg
268 °F
@Load 11.2 lb
rate 50°C/h
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 23 %23 %
Glow Wire Flammability Index 750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FAs Tested; Injection
Mold Temperature 70.0 °C158 °FAs Tested; Injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Novodur® HD M203FC G3 Acrylonitrile Butadiene Styrene (ABS)
Avient Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
Covestro Bayblend® FR 3311 TV PC/ABS Blend, 15% Glass Reinforced
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass

PMITSU9343 / 192007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.