MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ConocoPhillips Hydroclear® 46 Rock Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of pneumatic tool applications which require extreme-pressure properties for protection of equipment under high-load conditions, tackiness for good adhesion to working surfaces, good atomization with low-fogging tendencies and excellent low temperature fluidity. Hydroclear Rock Drill Oil is specifically formulated for use in surface-mining equipment, high- and low-speed drills, jackhammers, paving breakers, vacuum pumps, track-type air drills and other similar applications. Hydroclear Rock Drill Oil can also be used effectively as a saw guide lubricant in lumber mill applications. Hydroclear Rock Drill Oil is available in seven viscosity grades, ISO 32-320, to meet the needs of most applications and operating conditions. Hydroclear Rock Drill Oil exceeds the lubricant specifications for Ingersoll-Rand and Gardner-Denver drilling equipment.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.869 g/cc0.0314 lb/in³
Viscosity Measurement 115115Viscosity Index
Saybolt Viscosity at 100°F 236 SUS236 SUS
Saybolt Viscosity at 210°F 50 SUS50 SUS
Kinematic Viscosity at 40°C (104°F) 46 cSt46 cSt
Kinematic Viscosity at 100°C (212°F) 7.1 cSt7.1 cSt
ASTM Color 1.01.0
 
Mechanical PropertiesMetricEnglishComments
Falex Load Test 907000 g2000 lb
Timken Test 13600 g30.0 lb
 
Thermal PropertiesMetricEnglishComments
Pour Point -34.4 °C-30.0 °F
Flash Point 221 °C430 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Rock Elm Wood
Sodium Chloride, NaCl (Halite)
Overview of materials for Medium Alloy Steel
Overview of materials for Cast Stainless Steel
Lubriplate Rock Drill Oil Specialty Oil 10R and Fluid

WCON114 / 75151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.