MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Tecothane® Soft AR-62A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Clear Grade

Features: Medical Grade Soft Elastomeric TPUs with excellent resilience and recoverability, superior processability into complex shapes with ease and good mechanical properties

Process: Extrusion, Injection Molding or Solution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in(1”x.25”x6” bar); ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262ASTM D2240
Tensile Strength, Ultimate 10.3 MPa1500 psiASTM D412
Elongation at Break 720 %720 %ASTM D412
100% Modulus 3.10 MPa
@Strain 100 %
450 psi
@Strain 100 %
ASTM D412
200% Modulus 4.41 MPa
@Strain 200 %
640 psi
@Strain 200 %
ASTM D412
300% Modulus 5.38 MPa
@Strain 300 %
780 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.00524 GPa0.760 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 165 °C329 °FInjection
Front Barrel Temperature 170 °C338 °FInjection
Nozzle Temperature 160 °C320 °FInjection
Zone 1 188 °C370 °FExtrusion
Zone 2 193 °C379 °FExtrusion
Zone 3 199 °C390 °FExtrusion
Zone 4 204 °C399 °FExtrusion
Adapter Temperature 204 °C399 °FExtrusion
Die Temperature 199 °C390 °FExtrusion
Melt Temperature >= 171 °C>= 340 °FInjection
Mold Temperature 10.0 - 27.0 °C50.0 - 80.6 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane
Multibase TPSiV® 3011-50A Thermoplastic Silicone Vulcanizate
BASF Elastollan® S 50 A SPF TPUR
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane
CHT Group True Skin® 30 30 Shore A, Clear Addition Cure Material

PLUBR9111 / 203678

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.