MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemical Concepts Chem-Set™ 607 Clear Structural Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Crystal clear toughened adhesive for bonding a variety of plastics and metal substrates. Chem-Set 607 is a two-component, 100% reactive, toughened structural methacrylate adhesive specifically formulated for bonding wide variety of Plastic Surfaces.

FEATURES: -Crystal clear structural adhesive for assembly of plastic surfaces. -UV stable with self-leveling liquid. -Minimal or no surface preparation . -Room temperature cured with short open time. Applications: -Ideal for bonding Plexiglas PMMA, PETG, Polycarbonate, ABS, PVC, FRP, etc. -Ideal for Sign & Display industries. Plastic fabrication where clear bond-line is necessary.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0370 lb/in³
 1.04 g/cc0.0377 lb/in³
Viscosity 22000 - 28000 cP22000 - 28000 cPmixed
Brookfield Viscosity  10000 - 15000 cP
@Temperature 25.0 °C
10000 - 15000 cP
@Temperature 77.0 °F
Activator
 20000 - 25000 cP
@Temperature 25.0 °C
20000 - 25000 cP
@Temperature 77.0 °F
Adhesive
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D2240
Elongation at Break 5.0 %5.0 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flash Point 10.6 °C51.0 °FAdhesive
 10.6 °C51.0 °FActivator
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull
Working Life 6.00 - 8.00 min6.00 - 8.00 min
 
Descriptive Properties
ColorAdhesive: clear. Activator: off-white
Fixture Time12-14 minutes
Gap Fillingup to 0.015 inches
Mix Ratio10:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Saint-Gobain Normount® V2000 High-density Polyurethane Foam/High-performance Acrylic Adhesive Bonding Tape
Saint-Gobain CHR® SG13-03(R) High Performance Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® 2819-3(R) Acrylic Adhesive Zone Tape
Henkel Loctite® Output™ 384 Thermally Conductive Repairable Acrylic Adhesive

PCHEMI916 / 232168

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.