MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8255 HS PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and flexibility combined with excellent thermal and chemical resistance properties provided by the nylon backbone. It maintains its inherent chemical resistance to greases, oils and hydrocarbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³dry; ISO 1183
Water Absorption 1.2 %1.2 %24 hour; ISO Test
 7.1 %7.1 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.0 %2.0 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inASTM Data; MD
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8255 HS PA6 (Dry)
BASF Ultramid® 8253 HS PA6 (Conditioned)
BASF Capron® 1943 Impact Modified Nylon 6 (Dry)
Covestro Bayblend® M850 XF PC/ABS Blend
BASF Ultramid® 8253 PA6 (Conditioned)

PBASF9178 / 84942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.