MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omni Plastics OmniCarb™ PC/PBT 1020 FR0 PC/PBT
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Flame resistant; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Melt Flow 14 g/10 min14 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 61.0 MPa8850 psiASTM D638
Elongation at Break 45 %45 %ASTM D638
Flexural Strength 93.0 MPa13500 psiASTM D790
Flexural Modulus 2.413 GPa350.0 ksiASTM D790
Izod Impact, Notched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
@Thickness 3.17 mm
210 °F
@Thickness 0.125 in
ASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Omni Internal Testing
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 271 °C480 - 520 °F
Middle Barrel Temperature 249 - 277 °C480 - 530 °F
Front Barrel Temperature 249 - 277 °C480 - 530 °F
Nozzle Temperature 249 - 277 °C480 - 530 °F
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 26.7 - 82.2 °C80.0 - 180 °F
Drying Temperature 104 °C220 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Pocan® DP CF 2200 000000 PBT+PC
Envalior Pocan® KU 2-7604 000000 PBT+PC
Omni Plastics OmniCarb™ PC/PBT 400IM2 UV PC/PBT Alloy
Edinburg Plastics BCT505 PC/PBT
Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant

POMNI5124 / 185270

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.