MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

A. Schulman Matrixx FPP1A20CC Polypropylene Homopolymer, 20% Fiberglass Reinforced, Chemically Coupled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Data provided by The Matrixx Group, now a part of A. Schulman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inMatrixx internal test
Melt Flow 2.0 - 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 - 6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D2240
Tensile Strength, Yield 63.0 MPa9140 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Flexural Modulus 3.60 GPa522 ksiASTM D790
Izod Impact, Notched 0.600 J/cm
@Thickness 3.20 mm
1.12 ft-lb/in
@Thickness 0.126 in
ASTM D256
Gardner Impact <= 1.10 J<= 0.811 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C315 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C289 °FASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Matrixx Internal Test

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Thermofil P-20CC-0734A 20% Calcium Carbonate Reinforced
Asahi Kasei Thermofil P-40CC-1100 40% Calcium Carbonate Reinforced, Heat Stabilized Polypropylene
A. Schulman Matrixx CPP2B40 Polypropylene Copolymer, 40% Calcium Carbonate Filled
Asahi Kasei Thermofil P-40CC-0148 40% Calcium Carbonate Reinforced, Heat Stabilized Polypropylene
Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat

PMAT25 / 52410

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.