MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Abatron AboCast 8103-20 High-Performance Dielectric Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 8103-20 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is unique for its exceptional heat resistance and low dielectric constant.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³Part B
 1.17 g/cc0.0424 lb/in³Part A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.1 MPa9000 psi
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %
Tensile Modulus 3.07 GPa445 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cm
Dielectric Constant  2.7
@Frequency 60 Hz,
Temperature 100 °C
2.7
@Frequency 60 Hz,
Temperature 212 °F
 2.8
@Frequency 60 Hz,
Temperature 23.0 °C
2.8
@Frequency 60 Hz,
Temperature 73.4 °F
 3.0
@Frequency 60 Hz,
Temperature 150 °C
3.0
@Frequency 60 Hz,
Temperature 302 °F
Dissipation Factor  0.0070
@Frequency 60 Hz,
Temperature 100 °C
0.0070
@Frequency 60 Hz,
Temperature 212 °F
 0.0080
@Frequency 60 Hz,
Temperature 23.0 °C
0.0080
@Frequency 60 Hz,
Temperature 73.4 °F
 0.010
@Frequency 60 Hz,
Temperature 150 °C
0.010
@Frequency 60 Hz,
Temperature 302 °F
Arc Resistance >= 150 sec>= 150 sec
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C374 °FDeflection Temp at unknown load
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 100 °C
2.00 - 3.00 hour
@Temperature 212 °F
 60.0 - 240 min
@Temperature 120 - 160 °C
1.00 - 4.00 hour
@Temperature 248 - 320 °F
optional
Pot Life  30 min
@Temperature 80.0 °C
30 min
@Temperature 176 °F
 >= 480 min
@Temperature 25.0 °C
>= 480 min
@Temperature 77.0 °F
 
Descriptive Properties
Arc-Track Free (min)> 20002.5 KV
ColorClear
Parts by Weight (pbw)100Part A
 100Part B
Thermal Shock ResistanceScale 0 (poor) to 10 (excellent)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCast 8504-1 One-Component Epoxy
CENTROPLAST CENTROSOL Acrylonitrile butadiene Styrene copolymer
Abatron AboCast 8708-10 One-Component Structural/Dielectric Epoxy
Abatron AboCast 8103-30 High-Performance Dielectric Epoxy
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound

PABC897 / 107881

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.