MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zotefoams Plastazote® HL34 Polyethylene Foam
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0340 g/cc0.00123 lb/in³Nominal skin/skin; BS ISO 7214 1998
 0.0300 - 0.0390 g/cc0.00108 - 0.00141 lb/in³sheet density
Cell Length 0.400 - 1.10 mm0.0157 - 0.0433 in
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.00220 GPa0.319 ksiBS4370, part 4, method 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam
Zotefoams Plastazote® HL47 Polyethylene Foam
Zotefoams Plastazote® LD52 Low Density Polyethylene Foam
Zotefoams Plastazote® HD60 High Density Polyethylene Foam

PZOTEF953 / 150709

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.