Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 5456-H25
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95456; Aluminium 5456-H25; AA5456-H25; Al5456-H25
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0961 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 310 MPa45000 psiAA; Typical
Tensile Strength, Yield 165 MPa24000 psiAA; Typical
Elongation at Break 22 %
@Diameter 12.7 mm
22 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 71.0 GPa10300 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Shear Strength 187 MPa27100 psiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  22.1 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.3 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.9 µm/m-°C
@Temperature 20.0 - 100 °C
13.3 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.8 µm/m-°C
@Temperature 20.0 - 200 °C
13.8 µin/in-°F
@Temperature 68.0 - 392 °F
 25.9 µm/m-°C
@Temperature 20.0 - 300 °C
14.4 µin/in-°F
@Temperature 68.0 - 572 °F
Melting Point 568.3 - 638 °C1055 - 1180 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 568.3 °C1055 °FAA; Typical
Liquidus 638 °C1180 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °Fholding at temperature not required
Hot-Working Temperature 260 - 510 °C500 - 950 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.9 - 94.8 %91.9 - 94.8 %As remainder
Chromium, Cr 0.05 - 0.20 %0.05 - 0.20 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 4.7 - 5.5 %4.7 - 5.5 %
Manganese, Mn 0.50 - 1.0 %0.50 - 1.0 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5456-H116; 5456-H321
Aluminum 5456-H112
Aluminum 5456-H111
Aluminum 5456-H24
Aluminum 5456-O

MA5456H25 / 9287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.