MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg Emerson & Cuming Eccobond® 927-10 E Needle Bonding Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emerson & Cuming 927-10 E Eccobond® Needle Bonding Epoxy Adhesive
One component, fast curing, epoxy adhesive for needle bonding with polypropylene hubs. Also recommended for bonding sealing or insulating of heat sensitive parts. Cure Type: Heat Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³
Viscosity 11000 cP
@Temperature 25.0 °C
11000 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 9.65 MPa1400 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 120 °C
0.167 hour
@Temperature 248 °F
 15.0 min
@Temperature 100 °C
0.250 hour
@Temperature 212 °F
 18.0 min
@Temperature 90.0 °C
0.300 hour
@Temperature 194 °F
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant
Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System
Tra-Con Tra-Bond 927-1 Polysulfide Adhesive
Abatron AboWeld 8104-12 Polysulfide-Epoxy Sealant and Caulk

PEMERS77 / 35769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.