MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Trinseo EMERGE™ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Overview: EMERGE™ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processability of ABS, resulting in high toughness and high flow. This resin is suitable for use in a wide range of applications. EMERGE PC/ABS 7600 Natural has undergone biocompatibility testing based on ISO 10993 (Parts 5 & 10) and is suitable for use in medical equipment housings.

Main Characteristics:

  • Ignition-Resistant
  • Chlorine and Bromine Free
  • ISO 10993 (Parts 5 & 10)
Applications:
  • Medical equipment housings
  • Information technology equipment
  • Consumer electronics
  • Office and business equipment
  • Retail sales equipment

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 19 g/10 min
@Load 3.80 kg,
Temperature 230 °C
19 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118
@Thickness 3.20 mm
118
@Thickness 0.126 in
Injection Molded; ASTM D785
Tensile Strength at Break 44.1 MPa
@Thickness 3.20 mm
6400 psi
@Thickness 0.126 in
Injection Molded; ASTM D638
Tensile Strength, Yield 55.2 MPa
@Thickness 3.20 mm
8010 psi
@Thickness 0.126 in
Injection Molded; ASTM D638
Elongation at Break 80 %
@Thickness 3.20 mm
80 %
@Thickness 0.126 in
Injection Molded; ASTM D638
Elongation at Yield 4.0 %
@Thickness 3.20 mm
4.0 %
@Thickness 0.126 in
Injection Molded; ASTM D638
Tensile Modulus 2.69 GPa
@Thickness 3.20 mm
390 ksi
@Thickness 0.126 in
Injection Molded; ASTM D638
Flexural Strength 88.9 MPa
@Thickness 3.20 mm
12900 psi
@Thickness 0.126 in
Injection Molded; ASTM D790
Flexural Modulus 2.83 GPa
@Thickness 3.20 mm
410 ksi
@Thickness 0.126 in
Injection Molded; ASTM D790
Izod Impact, Notched 5.90 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
11.1 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 87.2 °C189 °FIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
@Thickness 3.20 mm
190 °F
@Thickness 0.126 in
Unannealed, Injection Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.2 °C
@Thickness 3.20 mm
171 °F
@Thickness 0.126 in
Unannealed, Injection Molded; ASTM D648
Vicat Softening Point 102 °C
@Load 1.02 kg
216 °F
@Load 2.25 lb
Rate B (120°C/h); ASTM D1525
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
Oxygen Index 31 %31 %ASTM D2863
Glow Wire Ignition Temperature 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index 950 °C
@Thickness 2.00 mm
1740 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 °C430 °FAim
 216 - 241 °C421 - 466 °F
Mold Temperature 60.0 - 71.1 °C140 - 160 °F
Drying Temperature 79.4 °C175 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Trinseo EMERGE™ PC/ABS 7700 NA Polycarbonate Resin
Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend
Trinseo CALIBRE™ 7100-15 Polycarbonate
Trinseo EMERGE™ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)

PZZDWST057 / 142266

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.