MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® HRP - 1/4 - 6.5 Fiberglass/Phenolic Honeycomb
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Core Material; Composite Fibers; Polymer; Thermoset; Phenolic

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This product was developed for use at service temperatures up to 350°F. However, it is also well suited for short exposures at high temperatures. The HexWeb® HRP-series honeycomb is available in the standard hexagonal configuration, as well as in the two formale geometries - OX-Core® and Flex-Core®.

Features: High strength up to 350°F; Good insulation and dielectric properties; Good bonding surface; Readily heat formed.
Applications: HexWeb® HRP has proven to be an excellent core material for radomes, aircraft structural parts and fairings, heat shields, and other assemblies that see elevated temperature service.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.104 g/cc0.00376 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength >= 5.52 MPa>= 800 psiBare, min
 >= 6.34 MPa>= 920 psiStabilized, min
 7.067 MPa1025 psiBare, typical
 8.14 MPa1180 psiStabilized, typical
Compressive Modulus 0.827 GPa120 ksiStabilized, typical
Shear Modulus 0.0896 GPa13.0 ksiPlate Shear, W Direction, typical
 0.159 GPa23.0 ksiPlate Shear, L Direction, typical
Shear Strength >= 1.79 MPa>= 260 psiPlate Shear, W Direction, min
 2.28 MPa330 psiPlate Shear, W Direction, typical
 >= 3.10 MPa>= 450 psiPlate Shear, L Direction, min
 4.00 MPa580 psiPlate Shear, L Direction, typical
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °FHigh strength retained

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexForce™ 1280 Fiber Glass Fabric
Hexcel® HexForce™ 7725 Fiber Glass Fabric
Henkel Hysol EA 9150 Composite Resin
Goodfellow E-glass/Epoxy Composite
Glassy Carbon used in heart valve prostheses

PHEXC407 / 98878

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.