MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Polystyrol® 158 K Polystyrene (Global)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).

Data was collected by ISO methods and provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Water Absorption 0.10 %0.10 %
Moisture Absorption at Equilibrium 0.10 %0.10 %
Linear Mold Shrinkage, Flow 0.0045 cm/cm0.0045 in/in
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 55.0 MPa7980 psi
Elongation at Break 3.0 %3.0 %
Tensile Modulus 3.30 GPa479 ksi
Charpy Impact Unnotched 1.70 J/cm²8.09 ft-lb/in²
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²
Tensile Creep Modulus, 1 hour 3300 MPa479000 psi
Tensile Creep Modulus, 1000 hours 2600 MPa377000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
 2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
Dissipation Factor  0.000050
@Frequency 1e+6 Hz
0.000050
@Frequency 1e+6 Hz
 0.000090
@Frequency 100 Hz
0.000090
@Frequency 100 Hz
Comparative Tracking Index 425 V425 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °F
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °F
Vicat Softening Point 101 °C214 °F
Glass Transition Temp, Tg 100 °C212 °F
Flammability, UL94 HB
@Thickness 3.18 mm
HB
@Thickness 0.125 in
Oxygen Index 18 %18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lacqrene® 3351(AS) Impact Polystyrene
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe)
BASF Procom® GC30H 251 Polypropylene
INEOS Styrolution Polystyrol 158 K GR 21 PS
Supreme Petrochem SP 6460 High Heat Polystyrene

PSF180 / 66761

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.