MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® LQ 2647 Polycarbonate, UV-Stabilized
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: UV-stabilized injection molding grade with easy mold release, suitable for spectacle glasses (LQ = Lens Quality).

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Moisture Absorption at Equilibrium 0.15 %0.15 %50% RH
Water Absorption at Saturation 0.35 %0.35 %
 0.35 %0.35 %
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
11 g/10 min
@Load 2.65 lb,
Temperature 572 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.0 MPa9140 psi
Elongation at Break >= 50 %>= 50 %Nominal
Elongation at Yield 6.0 %6.0 %
Tensile Modulus 2.40 GPa348 ksi
Charpy Impact Unnotched NBNB
Tensile Creep Modulus, 1 hour 2200 MPa319000 psi
Tensile Creep Modulus, 1000 hours 1900 MPa276000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm762 kV/in
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
Comparative Tracking Index 275 V275 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °F
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °F
Vicat Softening Point 143 °C289 °F
Glass Transition Temp, Tg 148 °C298 °F
Oxygen Index 26 %26 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586DIN 5026-1
Transmission, Visible 89 %
@Thickness 1.00 mm
89 %
@Thickness 0.0394 in
ISO 489-A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® LQ 2643 Polycarbonate, UV-Stabilized
IPB Veralite® 200 Transparent PETG Sheet
Covestro Apec® 2097 Polycarbonate
Changzhou Jinlibao GETAILONG JLB-110900 Clear PETG sheet
Plaskolite Mustang PETG Sheet

PBA469 / 26970

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.