Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber, 30% Filler by Weight Additive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance, Low Friction and Heat Stabilized Appearance: Black |