MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Mica Filler

Material Notes: Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in large area broad span applications where high modulus values are required and retained. Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Filler Content 20 %20 %ASTM D2584
Linear Mold Shrinkage 0.011 cm/cm
@Thickness 1.59 mm
0.011 in/in
@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min8.0 - 12 g/10 min230/2.16; May be specified; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D785
Tensile Strength at Break 31.63 MPa4588 psiASTM D638
Flexural Modulus 3.19 GPa462 ksiTangent; ASTM D790
Izod Impact, Notched 0.507 J/cm0.950 ft-lb/inAt 73°F; ASTM D256
Izod Impact, Unnotched 5.23 J/cm9.80 ft-lb/inAt 73°F; ASTM D256
Gardner Impact 0.451 J0.333 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced
Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black
Multibase Multi-Pro® 2005 M 20% Mica Filled Polypropylene

PPOLI020 / 56924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.