Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy Adhesive Filled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Excellent thermal shock resistance. Recommended for tube and radiator sealing. Cure Type: Heat Bonding Type: Epoxy The Eccobond® product line is now a part of Henkel; this specific grade is discontinued. |