MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyphenylene Ether, Heat Resistant
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Heat Resistant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.43 g/cc0.0379 - 0.0517 lb/in³Average value: 1.12 g/cc Grade Count:31
Moisture Absorption at Equilibrium 0.0600 - 0.100 %0.0600 - 0.100 %Average value: 0.0920 % Grade Count:10
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm0.00100 - 0.0100 in/inAverage value: 0.00588 cm/cm Grade Count:30
Melt Flow 1.00 - 50.0 g/10 min1.00 - 50.0 g/10 minAverage value: 18.1 g/10 min Grade Count:18
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104 - 121104 - 121Average value: 114 Grade Count:10
Tensile Strength, Ultimate 41.4 - 126 MPa6000 - 18300 psiAverage value: 65.6 MPa Grade Count:19
Tensile Strength, Yield 40.0 - 126 MPa5800 - 18300 psiAverage value: 62.4 MPa Grade Count:30
Elongation at Break 5.00 - 50.0 %5.00 - 50.0 %Average value: 31.8 % Grade Count:24
Elongation at Yield 1.50 - 8.00 %1.50 - 8.00 %Average value: 5.06 % Grade Count:8
Flexural Yield Strength 64.0 - 159 MPa9280 - 23000 psiAverage value: 90.9 MPa Grade Count:30
Flexural Modulus 2.06 - 9.65 GPa299 - 1400 ksiAverage value: 2.94 GPa Grade Count:31
Izod Impact, Notched 0.694 - 4.70 J/cm1.30 - 8.81 ft-lb/inAverage value: 1.86 J/cm Grade Count:31
 0.69407 - 1.6017 J/cm
@Temperature -40.0 - -30.0 °C
1.3003 - 3.0006 ft-lb/in
@Temperature -40.0 - -22.0 °F
Average value: 1.03 J/cm Grade Count:11
Charpy Impact, Notched 0.630 - 1.89 J/cm²3.00 - 8.99 ft-lb/in²Average value: 1.19 J/cm² Grade Count:9
Gardner Impact 14.1 - 22.6 J10.4 - 16.7 ft-lbAverage value: 17.7 J Grade Count:12
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 - 1.00e+17 ohm-cm1.00e+16 - 1.00e+17 ohm-cmAverage value: 2.59e+16 ohm-cm Grade Count:24
Surface Resistance 1.00e+16 ohm1.00e+16 ohmAverage value: 1.00e+16 ohm Grade Count:10
Dielectric Constant 2.80 - 2.902.80 - 2.90Average value: 2.88 Grade Count:10
Dielectric Strength 22.0 - 30.0 kV/mm560 - 762 kV/inAverage value: 26.3 kV/mm Grade Count:14
Dissipation Factor 0.000500 - 0.004000.000500 - 0.00400Average value: 0.00291 Grade Count:10
Arc Resistance 70.0 - 100 sec70.0 - 100 secAverage value: 80.0 sec Grade Count:10
Comparative Tracking Index 250 - 400 V250 - 400 VAverage value: 325 V Grade Count:4
Hot Wire Ignition, HWI 120 sec120 secAverage value: 120 sec Grade Count:4
High Amp Arc Ignition, HAI 60.0 - 120 arcs60.0 - 120 arcsAverage value: 90.0 arcs Grade Count:4
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minAverage value: 115 mm/min Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 - 80.0 µm/m-°C36.1 - 44.4 µin/in-°FAverage value: 74.0 µm/m-°C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 149 °C185 - 300 °FAverage value: 112 °C Grade Count:18
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 170 °C170 - 338 °FAverage value: 111 °C Grade Count:31
Vicat Softening Point 103 - 146 °C218 - 295 °FAverage value: 128 °C Grade Count:7
UL RTI, Electrical 65.0 - 110 °C149 - 230 °FAverage value: 81.4 °C Grade Count:14
UL RTI, Mechanical with Impact 65.0 - 110 °C149 - 230 °FAverage value: 81.4 °C Grade Count:14
UL RTI, Mechanical without Impact 65.0 - 105 °C149 - 221 °FAverage value: 77.7 °C Grade Count:14
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:28
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 320 °C428 - 608 °FAverage value: 259 °C Grade Count:10
Melt Temperature 171 - 316 °C340 - 600 °FAverage value: 263 °C Grade Count:18
Mold Temperature 37.8 - 120 °C100 - 248 °FAverage value: 75.0 °C Grade Count:25
Drying Temperature 70.0 - 110 °C158 - 230 °FAverage value: 93.8 °C Grade Count:28
Vent Depth 0.00254 - 0.00381 cm0.00100 - 0.00150 inAverage value: 0.00278 cm Grade Count:16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Ether, Impact Grade
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
Overview of materials for Polycarbonate, Molded

O4403 / 78321

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.