MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of general purpose, UV stable and low-temperature impact grades for use in a wide range of demanding applications and severe operating environments plus customized formulations to meet specialized requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.5 MPa6740 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 130 %130 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 70.7 MPa10300 psiASTM D790
Flexural Modulus 1.83 GPa265 ksiASTM D790
Izod Impact, Notched  5.30 J/cm
@Thickness 3.18 mm,
Temperature -40.0 °C
9.93 ft-lb/in
@Thickness 0.125 in,
Temperature -40.0 °F
Injection Molded; ASTM D256A
 6.90 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
12.9 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
@Thickness 6.35 mm
191 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 277 °C500 - 531 °F
Mold Temperature 65.6 - 87.8 °C150 - 190 °F
Drying Temperature 110 °C230 °F
Dry Time 2.00 hour2.00 hour
 
Descriptive Properties
AdditiveUV Stabilizer
FormsPellets
Generic MaterialPC+PBT
Generic NamePolycarbonate + PBT (PC+PBT)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond DIAMALOY 527 PC/PBT Alloy
Covestro Makroblend® UT3907 PC+PBT
Avient Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT)
Edinburg Plastics BCT505 PC/PBT
Edinburg Plastics CBI606 PC/PBT

PH0POL0717 / 145286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.