MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM class 25 Standard gray iron test bars, as cast
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: 987 kg transverse load on test bar.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.15 g/cc0.258 lb/in³Typical for Gray Cast Iron
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 174174
Hardness, Knoop 193193Converted from Brinell
Hardness, Vickers 181181Approximated. Converted from Brinell hardness.
Tensile Strength, Ultimate 179 MPa26000 psi
Modulus of Elasticity 79.0 - 102 GPa11500 - 14800 ksi
Ultimate Compressive Strength 669 MPa97000 psi
Poissons Ratio 0.290.29Calculated
Fatigue Strength 79.0 MPa11500 psiReversed bending fatigue limit
Shear Modulus 32.0 - 41.0 GPa4640 - 5950 ksi
Shear Strength 220 MPa31900 psiTorsional shear strength.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.25 - 3.5 %3.25 - 3.5 %
Chromium, Cr 0.050 - 0.45 %0.050 - 0.45 %
Copper, Cu 0.15 - 0.40 %0.15 - 0.40 %
Iron, Fe 91.9 - 94.2 %91.9 - 94.2 %As Balance
Manganese, Mn 0.50 - 0.90 %0.50 - 0.90 %
Molybdenum, Mo 0.050 - 0.10 %0.050 - 0.10 %
Nickel, Ni 0.050 - 0.20 %0.050 - 0.20 %
Phosphorus, P <= 0.12 %<= 0.12 %
Silicon, Si 1.8 - 2.3 %1.8 - 2.3 %
Sulfur, S <= 0.15 %<= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM class 30 Standard gray iron test bars, as cast
ASTM class 20 Standard gray iron test bars, as cast
Gray Cast Iron, ASTM A 48 Class 40
ASTM class 35 Standard gray iron test bars, as cast
Overview of materials for Gray Cast Iron

MCFE11 / 10405

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.