MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Polymers API 505 HF Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: API 505 HF is a high flow, intermediate grade of impact modified polystyrene. This material possess exceptional moldability and easy colorability. API 505 HF offers good retention of mechanical properties in applications with long flow length requirements.

Applications: API 505 HF is widely used in housewares, housings of all types, toys, displays and as base resin for color concentrate production.

Information provided by American Polymers, Inc.

Key Words: PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Melt Flow 14 g/10 min14 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 5959ASTM D785
Tensile Strength, Ultimate 26.2 MPa3800 psiASTM D638
Elongation at Break 45 %45 %ASTM D638
Tensile Modulus 2.00 GPa290 ksiASTM D638
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.17 mm
1.30 ft-lb/in
@Thickness 0.125 in
injection molded sample; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FAnnealed; ASTM D648
Vicat Softening Point 87.8 °C190 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Polymers API 375 Polystyrene
Overview of materials for Polystyrene, Impact Modified
Aclo Accucomp Polystyrene HS0600L High Impact
American Polymers API 550 Polystyrene
Bamberger Polymers Bapolan® 6403 Polystyrene, Extrusion

PAMER009 / 24010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.