MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmodur® BL 3475 BA/SN Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Diethyl malonate blocked, aliphatic polyisocyanate based on HDI / IPDI. In combination with Desmophen® grades to formulate lightfast, one-component stoving polyurethane coatings; as an additive in conventional stoving coating systems to improve the reactivity, flexibility and adhesion.

Properties / Applications; Desmodur® BL 3475 BA/SN is combined with polyols to formulate reactive, light-fast and weather-stable one-pack polyurethane stoving coatings. The main applications are in high-grade industrial finishes (can-/coil-coatings, etc.) and in primer surfacers for automotive OEM. Desmodur® BL 3475 BA/SN can also be used as an additive in conventional stoving systems to improve the reactivity, flexibility and adhesion.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccDIN EN ISO 2811
Viscosity 700 - 1300 cP700 - 1300 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesMetricEnglishComments
Flash Point 41.0 °C106 °FDIN 53 513/1
 
Descriptive Properties
Color<4Iod, DIN EN 1557
Content8.2%NCO content, blocked

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODURE® N 3390A BA/SN Polyurethane
Covestro DESMODURE® N 3368A BA/SN Polyurethane
Covestro Desmodur® Z 4470 SN/BA Polyurethane
Covestro Desmodur® Z 4470 SN Polyurethane
Covestro Desmodur® BL 4265 SN Polyurethane

PCOVEST0330 / 202113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.