MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 8223-30M300 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good appearance. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.

  • Neutral, easy coloring formulation.
  • Recommended for applications requiring excellent ozone resistance.
  • Used in sealing applications.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • EU and China RoHS compliant.
Applications:
  • Automotive – Grips, Interior and Interior Mat
Uses:
  • Automotive Applications
  • Automotive Interior Parts and Outdoor Applications
Processing Method: Injection Molding and Multi Injection Molding

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 28
@Thickness 2.00 mm
28
@Thickness 0.0787 in
15 sec; ISO 868
Tensile Strength at Break 8.48 MPa1230 psiAcross Flow; ASTM D412
Tensile Stress at Strain 5.60 MPa
@Strain 100 %
812 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 450 %450 %Across Flow; ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
 
Descriptive Properties
ColorNatural Color
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer
ExxonMobil Santoprene® 8221-85M300 Thermoplastic Elastomer
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer

PADVA021 / 22711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.