MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMET TIMETAL® 21S Titanium + Silicon Carbide Fiber Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: 4-Ply unidirectional laminate featuring SCS-6 silicon carbide fibers in titanium alloy matrix. Timet® 21S is a High-Strength, Oxidation Resistant Strip Alloy. 21S is well suited for metal matrix composites because it can be economically rolled to foil, is compatible with most fibers, and is sufficiently stable up to 816°C.

Data provided by TIMET.

Key Words: Beta 21S; UNS R58210; MMC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.24 g/cc0.153 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  517 MPa
@Temperature 816 °C
75000 psi
@Temperature 1500 °F
 1140 MPa
@Temperature 538 °C
165000 psi
@Temperature 1000 °F
 1720 MPa
@Temperature 21.1 °C
250000 psi
@Temperature 70.0 °F
Modulus of Elasticity 186 GPa27000 ksi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 816 °C1500 °F
Beta Transus 800 °C1470 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.5 - 3.5 %2.5 - 3.5 %
Carbon, C <= 0.050 %<= 0.050 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.40 %<= 0.40 %
Molybdenum, Mo 14 - 16 %14 - 16 %
Niobium, Nb (Columbium, Cb) 2.4 - 3.2 %2.4 - 3.2 %
Nitrogen, N <= 0.050 %<= 0.050 %
Oxygen, O 0.11 - 0.17 %0.11 - 0.17 %
Silicon, Si 0.15 - 0.25 %0.15 - 0.25 %
Titanium, Ti 76 - 80.8 %76 - 80.8 %Calculated as remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); ST 1500°F (816°C) + Age 1000°F (538°C)
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); 80% Cold Work
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); 40% Cold Work
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); 60% Cold Work
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3

NTIME21SX / 199564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.