MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 FR Hydraulic Fluid ISO Grade 100
Categories: Fluid; Lubricant

Material Notes: Description: Conoco FR Hydraulic Fluid is a fire-resistant, water-in-oil, invert-emulsion fluid for hydraulic systems, such as those found in underground mining equipment in which fire hazard and personnel safety concerns require water content for fire control. It is approved by the Mine, Safety, and Health Administration (MSHA) and the Factory Mutual Research Corporation (FMRC). FR Hydraulic Fluid is premixed and ready to use. It contains 40 vol. % water in oil. The oil provides a continuous outer layer to protect the hydraulic system from rust, corrosion and wear. The water provides excellent fire resistance in case of leakage. Thus, FR Hydraulic Fluid offers an extra margin of safety when compared to conventional petroleum hydraulic oils. FR Hydraulic Fluid is manufactured with high viscosity-index paraffinic base oils that are fortified with antiwear agents, biocides, rust and corrosion inhibitors and special emulsifiers that produce a stable, homogeneous mixture with a milky color. Proper system preparation is necessary if changing from a petroleum hydraulic oil or water-glycol fluid to FR Hydraulic Fluid. Avoid cork seals, as well as butyl seals and packing, because they tend to swell in service. Avoid filters and strainers on the pump inlet side of the system, as well as absorbent filters such as waste-packed or fuller's-earth units. Use paper filters only if the manufacturer can assure that they are compatible with water-containing fluids. To prevent excessive water loss, operate the system under 2000 psi pressure and do not allow temperatures to exceed 150°F (65°C). Most systems will run cooler with FR Hydraulic Fluid than with ordinary petroleum or synthetic fluids. The only special consideration is maintaining the proper water content, since water will be lost through evaporation. The MSHA requires a minimum of 40 vol. % water for adequate fire resistance. A stock solution is available for determining water content in the field.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³
pH 9.49.4
Viscosity Measurement 200200Viscosity Index
Saybolt Viscosity at 100°F 477 SUS477 SUS
Saybolt Viscosity at 210°F 92 SUS92 SUS
Kinematic Viscosity at 40°C (104°F) 103 cSt103 cSt
Kinematic Viscosity at 100°C (212°F) 18.5 cSt18.5 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.550 mm0.0217 in
 
Thermal PropertiesMetricEnglishComments
Melting Point -34.4 °C-30.0 °FFreezing point
Maximum Service Temperature, Air 65.6 °C150 °F
Pour Point -28.9 °C-20.0 °F
 
Descriptive Properties
ASTM Rust Test A & BPass
ColorMilky White
Slush point-2°F
Vickers 104°C Pump Test250Vane weight loss, mg.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 MV22 Super Hydraulic Oil
ExxonMobil 10W Mobil Hydraulic
ConocoPhillips Hydroclear® AW 46 Hydraulic Fluid
ChevronTexaco ECO® ISO 46 Hydraulic Oil AW
Unipetrol R2 Heavy Fuel Oil

WCON049 / 75086

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.