MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Rulon® 957 Bearing/Seal PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion. PTFE = polytetrafluoroethylene

957 Grade Bearing/Seal PTFE: Low friction/wear against coated metal or porcelain surfaces. Appropriate mating surfaces are steel, Rc 25 or higher, or painted metal/porcelain. Suitable for use in environments of steam, wet, dry, or vacuum type. Green in color. Material has electrical and thermal insulation properties.
Information provided by Saint Gobain Performance Products.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.25 g/cc0.0813 lb/in³ASTM D792
Water Absorption 0.00 %
@Time 86400 sec
0.00 %
@Time 24.0 hour
Immersion
Water Absorption at Saturation 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.2 MPa2200 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Compressive Yield Strength 6.89 MPa1000 psiMax load under tribological use
Coefficient of Friction, Dynamic 0.15 - 0.250.15 - 0.25Dry vs. Steel
Coefficient of Friction, Static 0.15 - 0.250.15 - 0.25Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec10000 psi-ft/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 112 µm/m-°C
@Temperature 25.6 - 93.3 °C
62.0 µin/in-°F
@Temperature 78.0 - 200 °F
Length
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature 25.6 - 93.3 °C
35.0 µin/in-°F
@Temperature 78.0 - 200 °F
Diameter
Maximum Service Temperature, Air 288 °C550 °F
Minimum Service Temperature, Air -240 °C-400 °F
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Rulon® 945 Bearing/Seal PTFE
Saint-Gobain Rulon® 123 Bearing/Seal PTFE
Saint-Gobain Rulon® 142 Bearing/Seal PTFE
Saint-Gobain Rulon® 1410 Bearing/Seal PTFE
Saint-Gobain Rulon® 641 Bearing/Seal PTFE

PSTGQZ172 / 68686

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.